Type
High Chromium electrode for high temperature applications.
classification
EN ISO
3581-A: E 25 4 R 32
W.Nr.
1.4820
Applications

CEWELD® 4820 AC is a cored wire alloyed, AC weldable stick electrode (Preferred =+) for production and repair welding on similar or similar, corrosion and heat resistant steels and steel castings. For furnaces requiring improved resistance to reducing and oxidizing sulfurous gases as well as for fi nal passes of weld joints. Scaling resistant up to 1100ºC.

Type
High Chromium electrode for high temperature applications.
Applications

CEWELD® 4820 AC is a cored wire alloyed, AC weldable stick electrode (Preferred =+) for production and repair welding on similar or similar, corrosion and heat resistant steels and steel castings. For furnaces requiring improved resistance to reducing and oxidizing sulfurous gases as well as for fi nal passes of weld joints. Scaling resistant up to 1100ºC.

Properties

CEWELD® 4820 AC is scale-resistant on the same base material and, due to its low nickel content, is resistant to attack by sulphur gases and oxidizing combustion gases up to 1100ºC. When welding CEWELD® 4820 AC, a low heat input is required, as alloys of this chemistry tend to become brittle at 600-800°C. The preheating temperature for similar and dissimilar steels should be 100 - 200ºC, depending on composition and material thickness. The interpass temperature should not exceed 300°C.

Classification
EN ISO
3581-A: E 25 4 R 32
FM
5
W.Nr.
1.4820
Suitable for

Mo-free 25Cr(Ni) alloys

1.4340, 1.4710, 1.4745, 1.4746, 1.4712, 1.4762, 1.4713, 1.4773, 1.4722, 1.4776, 1.4724, 1.4820, 1.4729, 1.4821, 1.4740, 1.4822, 1.4742, 1.4823

GX40CrNi27-4, G-X30CrSi6, G-X40CrSi23, X10CrSi6 502, X10CrAl24, X10CrAl7, X8Cr30, X10CrSi13, G-X40CrSi29, X8CrTi25, X10CrAl13, G-X12 CrSi 26 5, G-X40CrSi13, X20 CrNiSi 25 4, G-X40CrSi17, G-X40CrNi 25 4, X10CrAl18, G-X40CrNiSi 27 4,

AISI 327, 442, 446, ASTM A 297 HC

UNS S44200, 44600, J92605, J93005, J92605 

Approvals
CE
Welding positions
PA
PB
PC
PD
PE
PF
Redrying
300°C / 2 hr
Analysis
C Si Mn P S Cr Ni Mo N Cu Nb+Ta
0.1 1 2 0.02 0.01 26 5
Mechanical Properties
Heat
Treatment
RP0,2
(MPa)
Rm
(MPa)
A5
(%)
Hardness
As Welded 500 700 20 180 HB