- spécifications du produit
- conditionnement
- demander un devis
T92/P92 steel is commonly used at service temperatures up to 620°C. V, Nb and N additions provide this ‘creep strength enhanced ferritic’ (CSEF) alloy with improved high temperature creep resistance compared to standard CrMo creep resistant alloys.
P92, 9%Cr1.7%W0.5%Mo,
1.4901
X10CrWMoVNb 9 2
ASTM A213 Gr. T 92; A355 Gr. P92; A187 F92, A369 FP92; A1017 Gr 92
KA-STBA29; KA-STPA29 NF 616
YS = 390 MPa
E = 19 %
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
RT | |||||
730°C- 760°C 2h | 690 | 800 | 19 | 110 | HRc |