Extreme wear resistance even at higher temperatures. The deposit gives already a High hardness in the first layer. A buffer layer is recommended in case of sensible base material or old layers. Weldable without protective gas.Corresponding electrode: Dur 62 S
64-68 HRc hardfacing alloy, Cement, Mineral mixing, hammers, coke wear plates etc.
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
---|---|---|---|---|
As Welded | 67 HRc |