Type
Carbide powder, agglomerated and sintered
classification
EN ISO
14232-1 WC-Ni 88/12
Applications
carbide powder for wear resistant coatings produced by flame-, plasma or hig hvelocity- flame-spraying (HVOF). Tungsten-Carbide-Nickel-coatings are resistant to abrasion and oxidation. In comparison with WC-Co layers they show an improved corrosion resistance in aqueous solutions. Plasma sprayed coatings can achieve a hardness of up to 1000 HV0.1 and tensile strength acc. to DIN 50160 of 60 N/mm². The maximum operating temperature is 750°C.
Type
Carbide powder, agglomerated and sintered
Applications
carbide powder for wear resistant coatings produced by flame-, plasma or hig hvelocity- flame-spraying (HVOF). Tungsten-Carbide-Nickel-coatings are resistant to abrasion and oxidation. In comparison with WC-Co layers they show an improved corrosion resistance in aqueous solutions. Plasma sprayed coatings can achieve a hardness of up to 1000 HV0.1 and tensile strength acc. to DIN 50160 of 60 N/mm². The maximum operating temperature is 750°C.
Propriétés

Crystal size of WCApparent Density (ISO 3923-2)Particle Size Range in μmParticle Shape2.5 μm FSSS4.3 – 5.4 g/cm22/5 - 38/15 - 53/22Preponderant spherical 

Classification
EN ISO
14232-1 WC-Ni 88/12
Convient pour

Augers, impellors, shafts, hydraulics, pulling equipment, fan blades etc.

Positions de soudage
PC
Etuvage
Not required
Gas acc. EN ISO 14175
None
Analyse
Ni WC
12 88