- productspecificaties
- Verpakkingen
- vraag offerte
Higher productivity, higher deposition rates and improved wetting properties compared to solid wires with comparable analysis. Best to be used with CEWELD® FL 915 or CEWELD® FL 8111 welding flux.The deposit is resistant to seawater, thin acids and scale resistant in air and oxidizing gases up to 950°C. The weld deposit can be tempered.
1.4122, 1.4115 (G)X35CrMo17, 1.4313, 1.4000, 1.4001, 1.4002, Cast steels
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
---|---|---|---|---|
As Welded | 43 HRc |